Important facts about Ta7.5W alloy

Home > Knowledge > Important facts about Ta7.5W alloy

Ta7.5W alloy is prepared by powder metallurgy process.Due to the high interstitial element, it has a high strength at room temperature, and the Ta7.5W alloy wire has a yield strength of about 1100 MPa.


Physical properties:

Density:16.7g/cm3

Melting point:3025℃

Chemical properties:

Good corrosion resistance to strong acids such as sulfuric acid, hydrochloric acid, nitric acid and aqua regia

Application:

Ta-7.5w alloy is mainly used as spring material and other corrosion resistant elastic components in chemical corrosion equipment.